航空学报 > 1996, Vol. 17 Issue (3): 360-363

环境因素对三号航空有机玻璃应力-溶剂银纹的影响

史建立, 吴健, 过梅丽   

  1. 北京航空航天大学104教研室,北京,100083
  • 收稿日期:1994-07-09 修回日期:1994-12-08 出版日期:1996-06-25 发布日期:1996-06-25

EFFECT OF ENVIRONMENTAL FACTORS ON STRESS-SOLVENT CRAZING OF AVIATION ORGANIC GLASS YB-3

Shi Jianli, Wu Jian, Guo Meili   

  1. Faculty 104,Beijing University of Aeronautics and Astronautics,Beijing,100083
  • Received:1994-07-09 Revised:1994-12-08 Online:1996-06-25 Published:1996-06-25

摘要: 观测了三号航空有机玻璃 ( YB-3)在不同溶剂作用下的应力-溶剂银纹临界应力σc和银纹形貌。研究了吸水、紫外光辐照等单一环境因素和多个因素循环作用对 σc和银纹形貌的影响,并对影响机理进行了讨论

关键词: 航空工程, 聚甲基丙烯酸甲脂, 环境, 紫外辐射, 效应

Abstract: The critical stresses of stress\|solvent crazing,σ c,of a nonoriented aviation organic glass, YB-3(PMMA), were measured with various organic solvents and the craze morphology was observed. The effects of environmental factors such as water sorption, UV radiation, and their combination or cycling on σ c and the craze morphology were studied, and the influencing mechanisms were discussed.

Key words: aeronaut ical engineering, polymethyl methacrylate, environmentsult ravio, let radiation effects

中图分类号: