摘要: 通过试验认为微束等离子焊接钛合金薄板的保护问题,关键在于控制施焊时焊缝处于700℃以上的加热范围,和700℃到400℃的冷却时间。并论证了以氧的污染层厚度作为钛合金焊接污染程度判据的合理性。本文采用电子探针法对氧污染层厚度进行了测定,求出污染方程。从而。使微束等离子焊接钛合金薄板的污染问题,可通过调整焊接规范进行控制。

Abstract: This paper holds that the key to shielding during welding of titanium alloy sheets lies in the size of heating zone above 700℃ and the durarion of cooling to 400℃. The authors proved that it is rational to regard the oxide film as the mark of contamination of titanium ]alloy sheets and the the thickness of the oxide film as the criterion of the degree of contamination. Electron microprobe analyser was used to measure the thickness of the oxide film, and the equation relates the thickness of oxide film with heating temperature and holding time was obtained through data processing. Therefore, the degree of contamination during welding o’f titanium alloy sheets can be predicted and controlled through selecting welding methods and setting welding parameters.