航空锂电池非包容性热失控特定风险评估和安全边界分析

杨娟,李文静,王鹤然,刘冰洋,叶伟成,张青松,解江   

  1. 中国民航大学
  • 收稿日期:2026-07-30 修回日期:2026-10-02 出版日期:2026-10-08 发布日期:2026-10-08
  • 通讯作者: 杨娟
  • 基金资助:
    国家重点研发计划项目;深圳市科技计划资助项目

Particular risk assessment and safety boundary analysis of uncontained thermal runaway in aviation lithium-ion batteries

  • Received:2026-07-30 Revised:2026-10-02 Online:2026-10-08 Published:2026-10-08

摘要: 航空锂电池非包容性热失控作为新型特定风险源,所形成的高温喷射、火焰冲刷、颗粒物冲击和瞬态载荷等危害,严重威胁民机安全。本文建立了航空锂电池非包容性热失控后果评估模型,以机上结构板材材料、板厚和安装距离为关键安装与结构变量,从高温危害、冲击载荷以及两者耦合三方面进行分析,通过试验,获得迎火面与背火面峰值温度、穿孔面积、最大冲击力和主脉冲冲量等后果特征参数。结果表明,2A12航空铝板在5 cm安装条件下,板厚由1.0 mm增至3.0 mm时,背火面峰值温度由709.3 ℃降至161.2 ℃;在1.0 mm厚度、5 cm近距离工况下,2A12和6061板材发生贯穿性破坏,穿孔面积分别约为100 mm2和80 mm2;喷射冲击载荷具有短时、高峰值和距离敏感特征,最大冲击力由5 cm安装距离下的约205.45 N降至10 cm安装距离下的约102.45 N。采用高温风险、冲击风险和高温冲击耦合风险的非补偿式判定方法,形成C0—C3后果等级和板厚—距离风险边界,其中,近距离薄板工况是非包容性热失控后果最严重的主要风险区,增加板厚和安装距离均可有效降低后果等级,其中安装距离对冲击载荷衰减影响更为显著,板厚增加对背火面温升和贯穿性破坏具有明显抑制作用。研究结果可为航空锂电池特定风险评估的后果判定、局部防护结构设计和安装距离优化提供定量依据。

关键词: 航空锂电池, 非包容性热失控, 特定风险分析, 后果评估, 风险边界

Abstract: Uncontained thermal runaway of aviation lithium-ion batteries is an emerging particular risk source. The resulting hazards, including high-temperature jetting, flame impingement, particle impact, and transient loading, pose a serious threat to civil aircraft safety. In this study, a consequence assessment model for uncontained thermal runaway of aviation lithium-ion batteries was established. Structural plate material, plate thickness, and installation distance were selected as the key installation and structural variables, and the consequences were evaluated in terms of high-temperature hazards, impact loading, and their coupled effects. Experiments were conducted to obtain characteristic consequence parameters, including the peak temperatures on the fire-facing and back surfaces, perforation area, maximum impact force, and main-pulse impulse. The results show that, for the 2A12 aerospace aluminum plate at an installation distance of 5 cm, increasing the plate thickness from 1.0 mm to 3.0 mm reduced the peak back-surface temperature from 709.3 °C to 161.2 °C. Under the near-field condition of a 1.0 mm plate thickness and a 5 cm installation distance, the 2A12 and 6061 aluminum plates suffered through-thickness perforation, with perforation areas of approximately 100 mm2 and 80 mm2, respectively. The jet-induced impact load was characterized by short duration, high peak magnitude, and strong distance sensitivity, with the maximum impact force decreasing from approximately 205.45 N at 5 cm to 102.45 N at 10 cm. A non-compensatory assessment method integrating high-temperature risk, impact risk, and coupled high-temperature–impact risk was adopted to establish C0–C3 consequence levels and plate-thickness–distance risk boundaries. The near-field thin-plate conditions constituted the primary high-risk region with the most severe consequences. Increasing both plate thickness and installation distance effectively reduced the consequence level. Installation distance had a more pronounced effect on impact-load attenuation, whereas increasing plate thickness significantly suppressed back-surface temperature rise and through-thickness perforation. The results provide a quantitative basis for consequence classification in particular risk assessment, local protective-structure design, and optimization of installation distance for aviation lithium-ion batteries.

Key words: aviation lithium batteries, uncontained thermal runaway, particular risk analysis, consequence assessment, risk boundary