飞机快卸锁锁紧螺母重复使用特性
收稿日期: 2013-07-05
修回日期: 2013-10-26
网络出版日期: 2013-11-16
Characteristics of Prevailing Torque Nuts in Aircraft Latches Under Repeated Uses
Received date: 2013-07-05
Revised date: 2013-10-26
Online published: 2013-11-16
用于固定飞机表面快卸口盖的锁紧螺母在重复使用过程中容易发生松弛,使其拧出力矩减小,锁紧功能失效。首先从材料应变硬化、低周疲劳、接触面摩擦系数等方面对锁紧螺母最大拧出力矩的变化规律进行了定性分析。材料确定后,收口值的大小成为影响锁紧螺母重复使用特性的主要因素。试验研究中选定了3种不同收口值的锁紧螺母进行拧入拧出的重复使用试验,测量它们的最大拧出力矩。试验结果表明,随着重复使用次数的增加,螺母最大拧出力矩最初有一定波动,经历一段(N<200)恢复上升后,在重复使用次数200<N<1 500范围内,又缓慢下降趋于稳定;收口值对最大拧出力矩的下降速率有较大影响;获得了具有稳定符合规定最大拧出力矩的最优收口参数值。
王松伟 , 程小全 , 潘文 , 张纪奎 . 飞机快卸锁锁紧螺母重复使用特性[J]. 航空学报, 2014 , 35(3) : 788 -794 . DOI: 10.7527/S1000-6893.2013.0443
Prevailing torque nuts are widely used to fix the quick release covers on aircraft surfaces. But the unscrew torque decreases and locking mechanism may fail with repeated uses of the nuts. Parameters that may affect the maximum unscrew torque are first qualitatively analyzed which takes into consideration material strain hardening, low-cycle fatigue and frictional changes. The slotting gap value is considered to be a significant parameter that affects the repeated use characteristics when nuts of a specific material are fixed, and experiments are carried out to study it. Nuts with 3 different designed slotting gap values are screwed in and out to simulate the multiple reuses. The maximum unscrew torques are measured and torque-reuse curves are obtained. The test results show that, with the increase of reuse times, the maximum unscrew torque fluctuated at first, and, after a certain degree of recovery (a period of 50<N<200), decreased again slowly to a steady state during the region of 200<N<1 500.The slotting gap value affected the decrease rate and the best slotting gap value is obtained from the three tested designs.
[1] Wang X M, Bi S Q. A research on structure design for multiple seal packing for access doors on fighter airframe[J]. Aircraft Design, 2007, 27(4): 13-16. (in Chinese) 王向明, 毕世全. 飞机口盖复合垫片密封结构设计研究[J]. 飞机设计, 2007, 27(4): 13-16.
[2] Chinese Aviation Ministry of Industry. HB5639—1987 Hexagon slotting prevailing torque nuts (High temperature 230 ℃) [S]. 1987.(in Chinese) 中华人民共和国航空工业部. HB5639—1987 六角开槽锁紧螺母(最高工作温度230 ℃)[S]. 1987.
[3] Production Department and 694th Factory, Second Institute of Research, China Aerospace Industry Corporation. QJ 3079.1—1998 All metal prevailing torque nut[S]. Beijing: China Aerospace Industry Corporation, 1998.(in Chinese) 中国航天工业总公司第二研究院科研生产部和六九四厂. QJ 3079.1—1998 全金属锁紧螺母通用规范[S]. 北京: 中国航天工业总公司, 1998.
[4] China National Standardization Technical Committee of Fasteners. GB/T6184—2000 Prevailing torque type all-metal hexagon nuts, Style 1[S]. Beijing: Standard Press of China, 2000. (in Chinese) 全国紧固件标准化技术委员会. GB/T6184—2000 1型全金属六角锁紧螺母[S]. 北京: 中国标准出版社, 2000.
[5] China National Standardization Technical Committee of Fasteners. GB/T6185—2000 Prevailing torque type all-metal hexagon nuts, Style 2[S]. Beijing: Standard Press of China, 2000. (in Chinese) 全国紧固件标准化技术委员会. GB/T6185—2000 2型全金属六角锁紧螺母[S]. 北京: 中国标准出版社, 2000.
[6] Jiang Y, Zhang M, Park T, et al. An experimental investigation on frictional properties of bolted joints[C]//2002 ASME Pressure Vessels and Piping Conference. Vancouver, BC, Canada: ASME, 2002: 59-66.
[7] Eccles W, Sherrington I, Arnell R D. Frictional changes during repeated tightening of zinc plated threaded fasteners[J]. Tribology International, 2010, 43(4): 700-707.
[8] Zimandy A J C, Hess D P. Effect of reuse of locknuts with prevailing torque locking feature[J]. Journal of Failure Analysis and Prevention, 2013, 13(2): 121-127.
[9] Eccles W, Sherrington I, Arnell R D. Towards an understanding of the loosening characteristics of prevailing torque nuts[J]. Proceedings of the Institution of Mechanical Engineers, Part C: Journal of Mechanical Engineering Science, 2010, 224(2): 483-495.
[10] Bhattacharya A, Sen A, Das S. An investigation on the anti-loosening characteristics of threaded fasteners under vibratory conditions[J]. Mechanism and Machine Theory, 2010, 45(8): 1215-1225.
[11] Dinger G, Friedrich C. Avoiding self-loosening failure of bolted joints with numerical assessment of local contact state[J]. Engineering Failure Analysis, 2011, 18(8): 2188-2200.
[12] Wu R X, Wang Z L, Guo W D, et al. Fundamentals of mechanical design: Book 2[M]. 2nd ed. Beijing: Beihang University Press, 2005: 349-360. (in Chinese) 吴瑞祥, 王之栎, 郭卫东, 等. 机械设计基础: 下册 [M]. 2版. 北京: 北京航空航天大学出版社, 2005: 349-360.
[13] Wu F M. Fatigue strength[M]. Xi’an: Northwestern Polytechnical University Press, 1985: 30-40. (in Chinese) 吴富民. 结构疲劳强度[M]. 西安: 西北工业大学出版社, 1985: 30-40.
[14] Yu M Z, Zhang C. Handbook of steel products[M]. Beijing: Chemical Industry Press, 2010: 122-138. (in Chinese) 于民治, 张超. 钢铁产品手册[M]. 北京: 化学工业出版社, 2010: 122-138.
[15] Chen Z W. Study of cycle fatigue characteristics of materials[J]. Acta Aeronautica et Astronautica Sinica, 1988, 9(9): 445-450. (in Chinese) 陈志伟. 材料疲劳循环特性研究[J]. 航空学报, 1988, 9(9): 445-450.
[16] Pan W. Research on the life of self-locking nuts for airplane latches with quick-operating[D]. Beijing: School of Aeronautic Science and Engineering, Beihang University, 2010.(in Chinese) 潘文. 飞机快卸锁自锁螺母使用寿命研究[D]. 北京: 北京航空航天大学航空科学与工程学院, 2010.
[17] Ministry of Metallurgical Industry. GJB1951—1994 Specification for quality structure steel bars for aviation [S]. 1994.(in Chinese) 中华人民共和国冶金部. GJB1951—1994 航空用优质结构钢棒规范[S]. 1994.
[18] Aviation Industry Corporation of China. GJB2027—1994 General specification for quick-operating latch of aircraft [S]. 1994.(in Chinese) 航空工业总公司. GJB2027—1994 飞机快卸锁通用规范[S]. 1994.
/
〈 | 〉 |